TAPPI T 840 om-10

  • Testing Adhesives Used in Glued Lap Joints of Corrugated Fiberboard Containers
  • standard by Technical Association of the Pulp and Paper Industry, 01/01/2010
  • Publisher: TAPPI

$25.00$49.00


This method describes a procedure for evaluating the adhesive used in glued lap joints of corrugated containers. This method describes a laboratory procedure for evaluating glued lap adhesive applied to laboratory-prepared specimens made from the linerboard to be used in the manufacture of corrugated containers. A separate testing procedure for the finished containers is TAPPI T 813;Tensile Test for the Manufacturer's Joint of Fiberboard Shipping Containers.;This procedure measures heat resistance, water resistance, and cold resistance of the adhesive used in glued lap joints.

Related Products

TAPPI T 838 cm-03

TAPPI T 838 cm-03

Edge Crush Test Using Neckdown..

$33.00 $66.00

TAPPI T807-03

TAPPI T807-03

Bursting Strength of Linerboard..

$26.00 $51.00

TAPPI T 212 om-12

TAPPI T 212 om-12

One Percent Sodium Hydroxide Solubility of Wood and Pulp..

$25.00 $49.00

TAPPI T232 cm-01

TAPPI T232 cm-01

Fiber Length of Pulp by Projection..

$43.00 $85.00