• ASTM A608/A608M-06
Provide PDF Format

Learn More

ASTM A608/A608M-06

  • Standard Specification for Centrifugally Cast Iron-Chromium-Nickel High-Alloy Tubing for Pressure Application at High Temperature
  • standard by ASTM International, 09/01/2006
  • Publisher: ASTM

$26.00$52.80


1.1 This specification covers iron-chromium-nickel, high-alloy tubes made by the centrifugal casting process intended for use under pressure at high temperatures.

1.2 The grades of high alloys detailed in are intended for applications requiring strength and resistance to corrosion and scaling at high temperatures.

1.3 Optional Supplementary Requirements S1 to S11 are provided; these call for additional tests to be made if desired.

1.4 The values stated in either inch-pound units or SI units are to be regarded separately as standard. Within the text, the SI units are shown in brackets. The values stated in each system are not exact equivalents; therefore, each system must be used independently of each other. Combining values from the two systems may result in nonconformance with the specification.

Related Products

ASTM D7760-12

ASTM D7760-12

Standard Test Method for Measurement of Hydraulic Conductivity of Tire Derived Aggregates Using a R..

$22.00 $44.00

ASTM D2534-88(2012)

ASTM D2534-88(2012)

Standard Test Method for Coefficient of Kinetic Friction for Wax Coatings..

$20.00 $39.00

ASTM B249/B249M-14

ASTM B249/B249M-14

Standard Specification for General Requirements for Wrought Copper and Copper-Alloy Rod, Bar, Shape..

$30.00 $60.00

ASTM F1997-07

ASTM F1997-07

Standard Test Method for Determining the Sensitivity (Teasing) of a Tactile Membrane Switch (Withdra..

$23.00 $46.80